Modulated differential scanning calorimetry

Type of DSC (3.2.19) that enables reversible reactions to be distinguished from irreversible processes such as additional polymerization of the resin during the test.

Source: ISO 14692-1:2017, Petroleum and natural gas industries — Glass-reinforced plastics (GRP) piping — Part 1: Vocabulary, symbols, applications and materials, Second Edition, August 2017. Global Standards